P20+Ni Welding Wire

Material: P20+Ni / 1.2738 / 718H
Hardness: 33–38 HRC
🧊 Nickel-Alloyed Plastic Steel

Application: Specialized for large automotive bumper molds, TV cabinets, and high-gloss plastic injection tooling. Nickel addition ensures uniform hardness across thick sections and excellent photo-etching texturing.

P20+Ni TIG Welding Wire Sealed PP Tube Packaging
Sealed PP Tube Packaging
P20+Ni Laser Welding Wire Clean Surface Detail
Clean Wire Surface Detail

Select Welding Process & Diameters

Choose between Laser Welding or TIG Welding wire specifications.

0.15
mm
Spool / Rods
0.2
mm
Spool / Rods
0.3
mm
Spool / Rods
0.4
mm
Spool / Rods
0.5
mm
Spool / Rods
0.6
mm
Spool / Rods
Custom
Other Sizes
Contact Us →
0.8
mm
10 rods / tube
1.0
mm
10 rods / tube
1.2
mm
10 rods / tube
1.6
mm
10 rods / tube
2.0
mm
10 rods / tube
2.4
mm
10 rods / tube
Custom
Other Sizes
Contact Us →

TECHNICAL DATA SHEET (TDS) & PROCESS GUIDE Standard: AISI P20+Ni / DIN 1.2738 / GB 3Cr2NiMo

1. Chemical Composition (wt%)

Element C Si Mn Cr Mo Ni Fe
Specification 0.33–0.41 0.20–0.40 1.20–1.50 1.80–2.10 0.15–0.35 0.90–1.20 Balance

2. Welding Parameters: Laser vs. TIG

⚡ Laser Welding 0.15–0.6 mm

Preheat Temp No preheat required
Pulse Power 100–190 A
Shielding Gas Argon ≥99.99% (3–5 L/min)
HAZ Impact Ultra-narrow HAZ, zero sink marks

🔥 TIG Welding 0.8–2.4 mm

Preheat Temp 180°C – 220°C recommended
Welding Current 40–110 A (DCEN)
Shielding Gas Argon ≥99.99% (8–12 L/min)
Post-Heat Slow cooling in still air

💡 Key Repair & Operation Instructions:

  • Nickel Advantage: Addition of ~1.0% Nickel prevents soft spots and ensures uniform 33–38 HRC hardness even when welding deep cavities or thick-walled molds.
  • Photo-Etching & Texturing: Excellent graining and chemical etching compatibility, leaving no visible boundary halos.